IF you dont want to wait for some poxy-shield to arrive in the mail. I installed my sheer and chine in laminations with poxy-grip. I only applied to one side, there was lots of excess still that oozed all over so have a drop cloth underneath. I worked in halves. First glued and clamped the front half then mixed more epoxy and removed the last two clamps to ensure I coated every spot and then glued and clamped the rear half. I applied it with everything I could find, tongue depressors, little cheap rollers to sorta roll it out, helps to have two people.
_________________
My Zip build log...
http://www.vupilot.blogspot.comhttp://picasaweb.google.com/vupilot/Chr ... O0x7SvsQE#"Nothing screams poor craftsmanship like wrinkles in your duct tape."